| MOQ: | 1 PCS/20 Tons |
| Price: | $1300-3000 |
| Standard Packaging: | Customized based on project |
| Delivery Period: | 30-60 Days |
| Payment Method: | L/C,D/A,D/P,T/T |
| Supply Capacity: | 15,000 t / month |
Shot-blasted Sa 2.5 (Rz 40–75 µm) · Stripe-coated welds & edges · Inorganic zinc + silicone coat · CE & EN 1090-1
Sandblasting a boiler flue duct steel structure is surface engineering, not cosmetic prep. Flue support girders sit beside hot duct walls, sootblowers and moist fly-ash transitions. If mill scale stays on the plate or paint shrinks off sharp stiffener edges, coating failure starts in the first commissioning season.
![]()
Hot-rolled plates and H-sections arrive from the steel mill covered in blue-black iron oxide mill scale. Mill scale expands and contracts at a different rate from base Q355B steel during boiler start-up and shutdown cycles. Painting over intact or partially weathered mill scale traps a brittle layer underneath the primer. Once thermal cycling starts, the scale cracks and sheets of topcoat peel off together.
Calling a frame "sandblasted" without a standard number proves nothing. A functional boiler flue duct steel structure requires abrasive shot blasting to ISO 8501-1 Sa 2.5 (near-white metal, free of mill scale, rust and oil) combined with an anchor profile of Rz 40–75 µm so high-build primers interlock mechanically with the steel surface.
Blasting to Sa 2.5 exposes fresh, chemically reactive steel. In humid workshops, flash rust begins forming within hours—invisible under a rushed coat of primer, yet enough to cause premature blistering once the duct reaches operating heat.
Controlled fabrication shops prime blasted frames within a strict four-hour window under controlled atmospheric conditions:
Standard industrial workshop coatings—typically zinc-phosphate alkyd or standard two-pack epoxy—perform well at ambient plant temperatures. Above 120–150 °C, however, organic epoxy binders chalk, embrittle and delaminate.
Every boiler flue duct steel structure needs coating zones matched to actual surface temperature rather than one blanket paint spec:
Corrosion on power plant ducting almost never begins in the middle of a flat beam web. It begins on laser-cut edges, stiffener snipes, weld toes and punched bolt holes.
Liquid paint pulls away from sharp 90° plate edges by surface tension, leaving dry film thickness at the corner less than half of what a gauge reads on the flat flange. Before abrasive blasting, sharp sheared or thermal-cut edges on load-bearing gussets and duct stiffeners are ground to a minimum 2 mm radius (R ≥ 2 mm), and weld spatter or undercut is dressed smooth.
Immediately after the first blast pass or primer mist, a brush-applied stripe coat works primer into every weld seam, bolt hole rim, back-to-back angle gap and cope before full airless spraying proceeds.
Air preheater and flue duct supports carry wide sheet-metal casings under negative or positive draft pressure alongside heavy box beam buckstays and rolled H-section steel columns. Unlike static building girders, duct frames also connect to expansion joints and sliding shoes—following the same thermal-relief principles covered on our economizer support steel structure page.
All weld seams that require ultrasonic (UT) or magnetic particle (MT) testing are inspected and signed off before the frame enters the shot-blasting booth, so weld repairs never destroy finished coating integrity.
Coated steel frames scratch easily when bundled steel-on-steel with bare chains. Every boiler flue duct steel structure batch leaves our paint bay only after dry film thickness (DFT) logs and cross-cut adhesion checks confirm compliance with your project ITP.
Finished beams and buckstays are separated by timber battens and rubber or felt cushions inside 40 ft open-top or flat-rack containers; bolt kits, PTFE slide plates and small tie brackets travel in lined steel crates with waterproof erection tags matched to your drawing BoM.
We fabricate shot-blasted and coated boiler flue duct steel structure frames, buckstays, walkways and anchor templates strictly to client structural and shop drawings. Expansion bellows, damper blades, refractory insulation, civil foundations and site erection labour are excluded unless requested separately.
Send these engineering inputs for an itemized quotation:
![]()
Specify ISO 8501-1 Sa 2.5 (near-white metal, equivalent to SSPC-SP10) with an anchor profile of Rz 40–75 µm. Lower grades such as Sa 2.0 or manual wire brushing leave mill scale that blisters under boiler thermal cycling.
Conventional epoxy binders begin breaking down and chalking between 120 °C and 150 °C. Zones experiencing 150–400 °C surface heat require inorganic zinc silicate primer paired with a silicone heat-resistant topcoat.
Stripe coating is manual brush application of primer over weld toes, cut edges, bolt holes and crevices before full airless spraying. It prevents thin coverage caused by paint pulling back from sharp corners, stopping early rust at stiffener joints.
Yes. Magnetic dry film thickness (DFT) gauges check every structural zone against your coating schedule after full cure, and DFT inspection sheets ship alongside EN 10204 3.1 mill test certificates.
Cured members are separated with timber dunnage and non-abrasive padding, lifted with nylon webbing slings instead of bare wire rope, and braced securely inside 40 ft open-top or flat-rack containers.
Ultrasonic (UT) and magnetic particle (MT) weld testing are completed and signed off before full coating application. Inspecting welds early ensures any local grinding or repair re-enters the blast-and-prime cycle cleanly.
Send your structural drawings or BoM, steel grades, temperature zones, required coating DFT schedule, NDT percentage and destination port. Our estimating engineers review the drawings and return a detailed take-off and quotation.